  "material": "IG-110 核石墨",
  "uns": "",
  "property": "compressive_strength",
  "display_name": "抗压强度",
  "symbol": "Sc",
  "unit": "MPa",
  "variables": [
    {
      "name": "temperature",
      "unit": "°C",
      "label": "温度"
    }
  ],
  "observation_variables": [],
  "data_points": [
    {
      "inputs": {
        "temperature": 20.0
      },
      "observations": {},
      "y": 74.6
    },
    {
      "inputs": {
        "temperature": 300.0
      },
      "observations": {},
      "y": 65.5
    },
    {
      "inputs": {
        "temperature": 400.0
      },
      "observations": {},
      "y": 53.4
    },
    {
      "inputs": {
        "temperature": 500.0
      },
      "observations": {},
      "y": 40.9
    }
  ],
  "source_status": "public_measured_table",
  "source": {
    "title": "High Temperature Compressive Test of Nuclear Graphite IG-110",
    "url": "https://www.kns.org/files/pre_paper/7/401%EC%9D%B4%EC%98%81%EC%8B%A0.pdf"
  },
  "validity_note": "20–500 °C；单轴压缩试验典型点",
  "metadata": {
    "chart": {
      "x": "temperature",
      "type": "line"
    },
    "source_url": "https://www.kns.org/files/pre_paper/7/401%EC%9D%B4%EC%98%81%EC%8B%A0.pdf",
    "test_standard": "ASTM C695-21",
    "material_grade": "IG-110",
    "reference_temperature_C": 20.0
  },
  "note": "韩国核学会会议论文的 IG-110 高温压缩试验；ASTM C695 试样，20/300/400/500 °C。随温度升高，试验抗压强度下降。"
}